Lead concentrate is irreplaceable raw material used for the production of lead. The major markets are Poland, Germany, Romania and Bulgaria.
Lead concentrate (flotation galena) is produced in the process of flotation enrichment of zinc-lead ores. It contains max 9% of H2O. It is dark blue, its granulation ranges from 0-0,2mm and gravity is approx. 6g/cm3.
Content %
Pb | Zn | Ag | Cu | Cd | Bi | Sb | As | S | Sse4 | Fe | CaO |
55-72 | 1,5-2,5 | 0,0051 | 0,006 | 0,037 | 0,0001 | 0,04 | 0,1-0,21 | 18-25 | 0,25-0,4 | 7-12 | 0,5-1,2 |
SiO2 | Al2O3 | MgO | Mn | F | Cl | Co | Ni | Sn | Ge | Tl | H20 |
0,3-0,5 | 0,11 | 0,31 | 0,0056 | 0,001-0,005 | 0,0071 | <0,001 | <0,0015 | <0,001 | <0,001 | 0,0031 | 7-9 |
PKWIU 07.29.15.2, PCN-260700000
Annual analyzes 2018 - Content % | |||||||
![]() |
|||||||
Zn | Pb | PbO | Fe | SiO2 | CaO | MgO | Ss |
4,27 | 64,50 | 3,04 | 6,86 | 0,50 | 1,29 | 0,51 | 19,63 |
![]() |
|||||||
Cl | Cd | As | Sb | Ni | Co | Ag | F |
0,020 | 0,035 | 0,146 | 0,045 | 0,0016 | 0,0005 | 0,0091 | 0,0046 |